摘    要:采用Gleeble热模拟技术结合金相法对N80级ERW石油套管试制钢的连续冷却转变行为进行研究。试验表明,试制钢9#、10#试样在一般国内ERW焊管淬火冷却条件(20℃/s)下都无法获得完全马氏体组织,只有在≥50℃/s的高冷速条件下才能获得完全马氏体组织。10#试制钢的淬透性强于9#钢的。

Abstract: The characteristic of continuous cooling transformation of the experimental steel of N80 grade oil casing were studied by thermo mechanical simulator(Gleeble-3500).The results showed that the experimental steel of 9# and 10# could not transformed completely to martensite microstructure under the 20 ℃/s quenching condition of domestic ERW pipe welding.Only on the high cooling rate of above 50 ℃/s,the experimental steel could obtain whole martensite.The hardenability of the experimental steel 10# was stronger than that of 9#.

详情信息展示

N80级ERW石油套管用钢连续冷却转变行为的研究

李睿鑫1,王青峰2,陈辉3,贺飞3,尚成嘉4

(1.河北省秦皇岛市燕山大学亚稳材料科学与技术国家重点实验室
2.燕山大学 亚稳材料科学与技术国家重点室,河北秦皇岛 066004
3.北京科技大学 材料与工程学院,北京 100083
4.北京科技大学 材料科学与工程学院,北京 100083)

摘 要:采用Gleeble热模拟技术结合金相法对N80级ERW石油套管试制钢的连续冷却转变行为进行研究。试验表明,试制钢9#、10#试样在一般国内ERW焊管淬火冷却条件(20℃/s)下都无法获得完全马氏体组织,只有在≥50℃/s的高冷速条件下才能获得完全马氏体组织。10#试制钢的淬透性强于9#钢的。

关键词:电阻焊; N80; 级石油套管; 连续冷却转变; 淬透性

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号