Mechanical properties and microstructure of Fe-Al/Al2O3 composite with Cr, Mo and Ti
来源期刊:中国有色金属学报(英文版)2003年第4期
论文作者:李爱民 孙康宁 毕见强 尹衍升 张玉军
文章页码:860 - 863
Key words:Fe-Al intermetallic; Al2O3; composite; alloying element
Abstract: When Cr, Mo and Ti were added to Fe-Al/Al2O3 composite, the bending strength and fracture toughness of the composite were increased sharply. The highest value of bending strength can exceed 600MPa and the average value of fracture toughness exceed 12MPa·m1/2. With increasing content of Mo and Ti, the bending strength and fracture toughness both express the trend of increasing first and then decreasing. When the alloying elements were added to the composites the alloying extent is improved. The fracture mode of the composites are mainly transcrystalline.