用掺碳活化烧结技术制取碳化硼材料
来源期刊:中国有色金属学报2002年第6期
论文作者:王零森 尹邦跃 方寅初
文章页码:1210 - 1213
关键词:碳化硼; 活化烧结; 烧结活化剂
Key words:boron carbide; activated sintering; sintering activator
摘 要:研究了3种烧结活化剂(葡萄糖、 酚醛树脂和硬脂酸)和不同的掺碳量对碳化硼烧结的影响。发现活化剂葡萄糖优于其它两种活化剂, 以葡萄糖为活化剂, 掺碳3%, 在2270℃氢气中常压烧结1h获得的碳化硼材料密度为2.06g/cm3(相对密度82%), 这一密度高于文献中报道的采用相同粒度粉末制得的结果。
Abstract: The influences of carbon-doping activator (glucose, phenolic resin and stearic acid) and carbon-doping amount on sintered density of boron carbide were studied. It is discovered that glucose is much better than the others. A sintered density of 2.06g/cm3(82%TD) was obtained by doping 3% carbon using glucose as the activator precursor and pressureless sintering at temperature of 2270℃ for 1h in hydrogen. This density is higher than that of the literature reported using the powder with nearly the same particle size.