Effect of weld microstructure on weld properties in A-TIG welding of titanium alloy

来源期刊:中国有色金属学报(英文版)2003年第4期

论文作者:刘凤尧 杨春利 林三宝 吴林 苏生

文章页码:876 - 880

Key words:TIG welding; activating flux; penetration; microstructure; mechanical property

Abstract: Conventional TIG welding is known as its low productivity and limited weld depth in a single pass. Activating TIG welding (A-TIG) can greatly improve the penetration when compared with the conventional TIG welding. The effects of five kinds of activating fluxes with single component (NaF, CaF2, AlF3, NaCl or CaCl2) on penetration, microstructure and weld mechanical properties during the TIG welding of titanium alloy Ti-6Al-4V were studied. Compared with the conventional TIG welding, the experimental results show that the fluxes can greatly improve the penetration at the same welding specifications. This is because of the constriction of anode spots and the change of surface tension grads. Among them the effect of flux NaF is the best in the weld tensile strength, and the effect of flux CaF2 on the weld bend intension is the best. The appearance of inferior crystal grains and the structure of trident crystal grains are the main reasons that the performance of weld with fluoride is improved. These experimental results can be used as an aid for selecting suitable activating flux for titanium alloy.

详情信息展示

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号