In situ characterization of natural pyrite bioleaching using electrochemical noise technique

来源期刊:International Journal of Minerals Metallurgy and Materials2016年第2期

论文作者:Guo-bao Chen Hong-ying Yang Hai-jun Li

文章页码:117 - 126

摘    要:An in situ characterization technique called electrochemical noise(ECN) was used to investigate the bioleaching of natural pyrite.ECN experiments were conducted in four active systems(sulfuric acid,ferric-ion,9k culture medium,and bioleaching solutions).The ECN data were analyzed in both the time and frequency domains.Spectral noise impedance spectra obtained from power spectral density(PSD)plots for different systems were compared.A reaction mechanism was also proposed on the basis of the experimental data analysis.The bioleaching system exhibits the lowest noise resistance of 0.101 MΩ The bioleaching of natural pyrite is considered to be a bio-battery reaction,which distinguishes it from chemical oxidation reactions in ferric-ion and culture-medium(9k) solutions.The corrosion of pyrite becomes more severe over time after the long-term testing of bioleaching.

详情信息展示

In situ characterization of natural pyrite bioleaching using electrochemical noise technique

Guo-bao Chen,Hong-ying Yang,Hai-jun Li

School of Metallurgy, Northeastern University

摘 要:An in situ characterization technique called electrochemical noise(ECN) was used to investigate the bioleaching of natural pyrite.ECN experiments were conducted in four active systems(sulfuric acid,ferric-ion,9k culture medium,and bioleaching solutions).The ECN data were analyzed in both the time and frequency domains.Spectral noise impedance spectra obtained from power spectral density(PSD)plots for different systems were compared.A reaction mechanism was also proposed on the basis of the experimental data analysis.The bioleaching system exhibits the lowest noise resistance of 0.101 MΩ The bioleaching of natural pyrite is considered to be a bio-battery reaction,which distinguishes it from chemical oxidation reactions in ferric-ion and culture-medium(9k) solutions.The corrosion of pyrite becomes more severe over time after the long-term testing of bioleaching.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号