Ding11. National Engineering Research Center of Light Alloy Net Forming and Key State Laboratory of Metal Matrix Composite,School of Materials Science and Engineering,Shanghai Jiao Tong University2... of dual-phase Mg-8Li-3Al-2Zn-0.5 Y(wt%) alloy, which was prepared by casting, and then homogenized and rolled at 200℃. The rolling process was conducted with 10% reduction per pass and five different......
J. Cent. South Univ. (2018) 25: 1573-1581 DOI: https://doi.org/10.1007/s11771-018-3849-x Derivation and application of concentration formula of alloy genes of DO3-type in BCC alloy systems PENG... and Engineering, Central South University, Changsha 410083, China Central South University Press and Springer-Verlag GmbH Germany, part of Springer Nature 2018 Abstract: Taking Ta–W alloy system......
alloys decrease with increasing lithium, while the ductility increases apparently; the damping capacity of Mg-Li-Al alloys increases with the rises in temperature and lithium content. For Mg8Li1Al alloy, the damping capacity can go up to 0.01. The higher damping capacity of Mg-8Li-1Al alloy may contribute to the interface damping between α (Mg) and β (Li) phases. Keyword:
......
......
......
J. Cent. South Univ. (2012) 19: 2073-2080 DOI: 10.1007/s11771-012-1247-3 Hot-compression behavior of Al alloy 5182 TANG Jian-guo(唐建国), HUANG Xing-xing(黄星星), ZHANG Xin-ming(张新明) School of Materials Science and Engineering, Central South University, Changsha 410083, China ? Central South University Press and Springer-Verlag Berlin Heidelberg 2012 Abstract: Hot-compression of aluminum alloy 5182......
Microstructure evolution of TA15 titanium alloy during hot power spinningCHEN Yong, XU Wen-chen, SHAN De-bin, GUO Bin(School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China)Abstract:The microstructure evolution of TA15 titanium alloy during hot power spinning was studied. Effects of wall reduction on microstructure evolution of TA15 titanium alloy were......
......
. The as-cast alloy was composed of α-Mg, β-Li, AlLi, Al2Y and MgAlLi2 phases. Annealing of the cold rolled alloy at 350 °C for 60 min was considered to be optimum. This caused full static recrystallization... Mg-8Li-3Al-0.4Y alloy. Previous work [13] suggested that the Mg-8Li-3Al-0.4Y alloy consisted of the five phases: α-Mg, β-Li, AlLi, Al2Y and MgAlLi2. In addition, small whitish grains of the Mg-rich α......