Oxidation of Al2O3-30%TiCN-0.2%Y2O3 Composite Yan Changhao1,Li Xikun2,Xiu Zhimeng3,SUN Xudong3,QIU Guanming1,Dai Shaojun1 (1.Nanjing University of Technoloy, Nanjing 210009, China;2.Shenyang... 130022, China) Abstract:The oxidation behavior of Al2O3-30%TiCN-0.2%Y2O3 composite and its effect on high temperature bending strength was studied. The result indicates that the mass gain during......
......
The Studies of Composite Electroless Plating Process on Sintering Ndfeb Permanent Magnet MENG Yong-qiang1,MA Jing1,HU Jian-wen1,YAN Dong-Qing1,GAO Qing1 (1.School of material, Hebei University... in neutral bath (PH=7) for 40min and in acidic bath (PH=4.8~5.1) for 2h. A composite electroless plating with different phosphor content was obtained. The results show that the composite plating coatings......
Synthesis and electrochemical performance of Co3O4/C composite anode for lithium ion batteries GUO Hua-jun(郭华军), SUN Qian-ming(孙乾铭), LI Xin-hai(李新海), WANG Zhi-xing(王志兴), PENG Wen...; Abstract: The Co3O4/acetylene black composite anodes were......
......
SUPERPLASTICITY IN SiCw/ZK60 COMPOSITE M.Zhao1,F.Yan1,K.Wu1 (1.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin,150001, China) Abstract:The superplastic deformation behavior of SiCw/ZK60 composite was investigated at temperatures ranging from 573K to 723K and at initial strain rates ranging from 8.3× 10-4 S-1 to 8.3× 10-2 S-1. A maximum elongation of 200......
......
Oxidation behavior of Fe40Al-xWC composite coatings obtained by high-velocity oxygen fuel thermal spray XIANG Jun-huai(向军淮)1, 2, 3, ZHU Xing-he(朱星河)1, CHEN Gang(陈 钢)1, DUAN Zhi(段 智)1... into the oxidation behavior of the as-deposited coatings at 650 ℃ under 0.1 MPa flowing pure O2. The present results show differences in the oxidation behavior of Fe40Al coating and Fe40Al-xWC composite coatings......
......