共搜索到17259条信息,每页显示10条信息,共1726页。用时:0小时0分0秒595毫秒
......
物在熔融NaCl-KCl中的溶解度[12-13] Fig. 9 Common metal solubility in molten NaCl-KCl[12-13] 图10 Co基合金在熔融NaCl-52%MgCl2中的腐蚀机理 Fig. 10 Corrosion mechanism of Co-based alloys 3.3 残盐的成分分析 腐蚀... of metal chloride. Key words: molten salt; corrosion; Co-based alloy; NaCl-52%MgCl2 Foundation item: Project(51441003) supported by the National Natural Science Foundation of China; Project......
develop new preparation technology of titanium which is low cost, short process flow and environmentally friendly. Electro-deoxidization of titania in molten salt is a novel method to prepare metal.... Although the metal layer of the pallets sintered at 750 ℃ has the maximum thickness, but it’s intensity is so poor that it is incline to be pulverized by molten salt. So 900 ℃ is the optimal sintering......
高温金属腐蚀-磨损试验机示意图 Fig. 1 Schematic diagram of high temperature test rig for corrosion-wear in molten metal 图2 摩擦副的形状及尺寸 Fig. 2 Shape and dimension of friction pair (Unit: mm) 2...属研究所, 2000: 73-96.HUANG Xu-qiang. Study on materials with corrosive wearing resistance to ceramics in molten zinc-aluminum alloy[D]. Shenyang: Institute of Metal Research Chinese Academy of Sciences......
complex ions was inhibited, and a large dendrite Hf metal was achieved in molten salt electrorefining.关键词:...Electrochemistry of Hf(Ⅳ) in NaCl–KCl–Na –K2HfF6 molten saltsYan-ke Wu,Guo-qing Yan,Song Chen,Li-jun Wang摘 要:The cathodic reduction mechanism of Hf(Ⅳ) ions......
structures are in reasonable agreement with the experimental ones. Key words: Al-Fe alloy; molten structure; medium range order CLC number: TG146; TG111 Document code: A 1 INTRODUCTION...) peak. Sometimes the prepeak in the structure of molten alloys was neglected[2]. Homtova et al[3] suggested that prepeak was indicative of fragments of crystalline Fe2Al5 compound in the liquid Al-Fe......
nanocoating methods. The molten salt method may also be used to produce other metal oxides coating nanostructures as the electrode materials for lithium-ion batteries. Key words: nanometer materials...Trans. Nonferrous Met. Soc. China 25(2015) 3651-3656 Synthesis of α-Fe2O3@SnO2 core-shell nanoparticles via low-temperature molten salt reaction route Gang LIU1,2, Wei-jia SUN2, Sha-sha TANG3, Shu......
behavior on carbon surface by molten melts (molten melts, liquid metal or alloy) play a critical role in developing high-temperature energy storage and transfer technique, material casting and processing, metal production by electrolysis in molten salts and carbon materials production by molten salts carbonization and activation. However, thus far, the systematic reviews focus on this subject......
of cerium metal from molten fluoride systems.The cathodic process of Ce3+ ions in LiF-NaF and LiF-NaF-CaF2 molten salts was studied using electrochemical techniques as steady state and cyclic...Electrochemical studies on cerium(Ⅲ) in molten fluoride mixturesVIRGIL CONSTANTIN,ANA-MARIA POPESCU,MIRCEA OLTEANURomanian Academy,Institute of Physical Chemistry "Ilie Murgulescu",Department......
of cerium metal from molten fluoride systems.The cathodic process of Ce3+ ions in LiF-NaF and LiF-NaF-CaF2 molten salts was studied using electrochemical techniques as steady state and cyclic...Electrochemical studies on cerium(Ⅲ) in molten fluoride mixturesVIRGIL CONSTANTIN,ANA-MARIA POPESCU,MIRCEA OLTEANURomanian Academy,Institute of Physical Chemistry "Ilie Murgulescu",Department......