. ZHANG Yi-wen, LIU Jian-tao. Development in powder metallurgy superalloy[J]. Materials China, 2013, 32(1): 1-11. [2] GARIBOVG S, GRITS N M. The way of creatingnewhigh strengthpowder metallurgy superalloy..., LIU Ming-dong, LIU Jian-tao. Fracture character of low cycle fatigue of P/M superalloy FGH97[J]. Acta Metallurgica Sinica, 2010, 46(4): 444-450. [5] 刘新灵, 陶春虎. 粉末高温合金缺陷特性及寿命预测方法研究进展和思考[J]. 材料导报, 2013......
Influence of phosphorus on oxidation behavior oflow thermal expansion superalloy IN909 at 650 ℃ SUN Ya-ru(孙雅茹)1, 2, SUN Wen-ru(孙文儒)2, HOU Gui-chen(侯桂臣)2, GUO Shou-ren(郭守仁)2, LIU Zheng (刘 正)1, HU... to the oxidation layer. Key words: IN909 alloy; low thermal expansion superalloy; oxidation; phosphorus 1 Introduction Low thermal expansion superalloys are helpful to improve the efficiencies of aero......
-treated Ni-based cast superalloy IN792 were investigated. The results show that M5B3 boride precipitates at the grain boundary. A special orientation relationship between M5B3 phase and the matrix at one......
Oxidation Behavior of the Nickel-Based Superalloy DZ125 at 980℃Ye-Bing Hu1,Li Zhang2,Cong-Qian Cheng1,Peng-Tao Zhao2,Guang-Ping Guo2,Jie Zhao11. School of Materials Science and Engineering, Dalian University of Technology2. Beijing Institute of Aeronautical Materials摘 要:The isothermal oxidation behavior of the nickel-based superalloy DZ125......
Superplastic behavior of a powder metallurgy superalloy during isothermal compressionLiming Tan1,2,3,Yunping Li1,2,3,Feng Liu1,2,3,Liang Jiang1,2,31. State Key Laboratory of Powder Metallurgy,Central...">In this work,the flow behaviors and microstructure evolution of a powder metallurgy nickel-based superalloy during superplastic compression is investigated.Based on the strain rate sensitivity m......
and microstructural characteristics, mechanical properties, chemical and physical properties, hot and cold workabilities, and application characteristics. Key words: superalloy; turbine disc superalloy GH2135; turbine ring part superalloy GH2035A; turbine blade superalloy DZ417G; superheater tube superalloy GH2984; hot corrosion resistant superalloy; K444; K435; K452; GH4413 高温合金具有良好的高温强度和抗氧化抗腐蚀性能,优异的抗疲劳和抗蠕变性能......
......
superalloy has excellent mechanical properties at intermediate temperature. The refinement mechanism was discussed.关键词:......
THE EFFECT OF BORON AND CARBON ADDITION ON WELDABILITY OF DS TMS-75 SUPERALLOY M.C.Chaturvedi1,Y.L.WANG1,N.L.Richards1 (1.Department of Mechanical and Industrial Engineering, University of Manitoba... alloys. Key words:Ni-based superalloy; low melting point constituents; liquation cracking; [全文内容正在添加中] ......
PHASE TRANSFORMATION AND CHARACTERISTICS IN FRECKLE AREAS FOR INCONEL 625 SUPERALLOY Y.P.Zeng1,X.S.Xie1,J.X.Dong1,M.C.Zhang1 (1.University of Science and Technology Beijing, Beijing 100083, China... and liquid segregation calculation can give a reasonable interpretation of the freckle feature for this alloy. Key words:freckle; superalloy; Inconel 625; thermodynamic calculation; [全文内容正在添加中] ......