共搜索到21655条信息,每页显示10条信息,共2166页。用时:0小时0分0秒736毫秒
Numerical simulation of continuous roll-casting process of aluminum alloy XIE Shui-sheng(谢水生), YANG Hao-qiang(杨浩强), HUANG Guo-jie(黄国杰) State Key Laboratory for Fabrication and Processing of Non... of continuous roll-casting process (CRP) of aluminum alloy, the investigations of the flow behavior within the metal pool, the heat transfer condition between roll and strip, the pouring temperature......
Compressive formability of 7075 aluminum alloy rings under hydrostatic pressure LIU Gang(刘 钢), WANG Li-liang(王礼良), YUAN Shi-jian(苑世剑), WANG Zhong-ren(王仲仁) School of Materials Science... of the ring, numerical simulation and experimental research were carried out. The effect of hydrostatic pressure on the deformation of aluminum alloy 7075 ring was obtained by numerical simulation......
Joint performance of laser-TIG double-side welded 5A06 aluminum alloy CHEN Yan-bin(陈彦宾), MIAO Yu-gang(苗玉刚), LI Li-qun(李俐群), WU Lin(吴 林) State Key Laboratory of Advanced Welding Production... of the welds of laser-TIG double-side welded 5A06 aluminum alloy was investigated. The results show that the weld cross-sectional shape has an intimate relation with the mechanical properties......
Portevin-Le Chatelier effect in Al-Zn-Mg-Cu-Zr aluminum alloy CHEN Jun-zhou(陈军洲)1, 2, ZHEN Liang(甄良)1, FAN Li-wei(樊立伟)3, YANG Shou-jie(杨守杰)2, DAI Sheng-long(戴圣龙)2, SHAO Wen-zhu(邵文柱)1...; Abstract: Portevin-Le Chatelier (PLC) effect in a severely cold-rolled Al-Zn-Mg-Cu-Zr aluminum alloy (AA7055 type) plate before and after......
Dynamic softening behaviors of 7075 aluminum alloy QUAN Guo-zheng(权国政)1, LIU Ke-wei(刘克威)1, ZHOU Jie(周 杰)1, CHEN Bin(陈 斌)2 1. School of Material Science and Engineering, Chongqing University... hot deformation of 7075 aluminum alloy were studied by isothermal hot compression tested at temperatures of 250, 300, 350, 400 and 450 ℃ and strain rates of 0.01, 0.1, 1 and 10 s-1 on Gleeble1500......
Defect analysis of complex-shape aluminum alloy forging SHAN De-bin(单德彬), ZHANG Yan-qiu(张艳秋), WANG Yong(王 勇), XU Fu-chang(徐福昌), XU Wen-chen(徐文臣), L? Yan(吕 炎) School of Materials Science... aluminum alloy with complex shape. The complexity of forging is easy to lead to the occurrence of the defects, such as underfilling, folding, metal flow lines disturbance and fibre breaking. The reasons......
surface is limited. It is acknowledged that aluminum foam is a kind of closed cell porous metal, so gas is enclosed in each independent cell. Accordingly, we believe that bubble surface cannot react..., the critical oxygen volume fraction needed to produce aluminum foams with good cell structure and the role of oxide film in foam stability have not been reported. In order to improve the gas injection foaming......
......
Investigation of Out-Phase Electromagnetic Casting of Aluminum Alloy () 摘要:The influences of out-phase electromagnetic field on the as-cast structure of horizontal direct chill casting aluminum... changes from columnar grains to equiaxed grains and grain size decreases. 关键词:out-phase electromagnetic field; aluminum alloy; horizontal direct chill casting; as-cast structure; [全文内容正在添加中] ......
......