A review of composition evolution in Ni-based single crystal superalloysWanshun Xia1,Xinbao Zhao1,Liang Yue1,Ze Zhang21. Institute of Superalloys Science and Technology, School of Materials Science... crystal superalloys(Ni-SXs) are extensively applied in modern aero-engine and industrial gas turbine. Apart from the special single crystal structure which is disadvantageous to extension of creep......
......
Weakening Mechanisms of Platelike σ Phase on Ni-base Superalloys刘跃生,赵先国,刘志中,谢锡善摘 要:<正> On the basis of an investigation on σ phase inNi-base cast superalloy K24 and the results aboutσ phase in other Ni-base superalloys,an embrittl-ing mechanism and a softening mechanism,bywhich platelike σ phase weakens the Ni-basesuperalloys,have been proposed.It......
J. Cent. South Univ. (2020) 27: 1395-1403 DOI: https://doi.org/10.1007/s11771-020-4375-1 Catalytic effect of silver-bearing solid waste on chalcopyrite bioleaching: A kinetic study LIAO Rui(廖蕤)1, 2... using silver-bearing solid waste under different chalcopyrite/solid waste ratios. Bioleaching behavior indicates that silver-bearing solid waste can enhance the bioleaching process, and the redox......
THE ROLE OF NIOBIUM IN NICKEL-BASED SUPERALLOYS AND CHARACTERIZATION OF PM ALLOY EP741NP T. Carneiro1,D. Furrer2,J. Radavich3 (1.Reference Metals Co., Bridgeville, PA 15017, USA;2.Ladish Go., Inc., Gudahy, WI 53110, USA;3.Micro-Met Laboratories, West Lafayette, IN 47906, USA) Abstract:The role of niobium in nickel-based superalloys is reviewed. The importance of niobium as a strengthener......
Study on the Hydrate Activity of Fine Building Waste邢伟宏摘 要:<正>This paper discusses the way to activate building waste in order to increase the amount of waste used in building material products. Different admixtures are studied. The results show that the strength of hardened cement mortar with admixtures is higher than that without admixtures......
to the result. Key words: L12 type intermetallic compound; phase equilibrium; Co-Ti-Ta; Co-based superalloys 1 Introduction The development of superalloys has been driven by the demand to increase... Co-based and Ni-based superalloys, and it has been known that Ta can stabilize the γ′ phase [1-5]. However, both γ′-Ni3Ta and γ′-Co3Ta are not stable, thus, a quantitative thermodynamic description......
......
Recovery of Iridium from Waste Zirconia Sand季彩霞,朱积寿,汪炳瑞摘 要:RecoveryofIridiumfromWasteZirconiaSandJiCaixia,ZhuJishouandWangBingrui(季彩霞)(朱积寿)(汪炳瑞)GeneralResearchInstituteforNonferrousMet...关键词:......
J. Cent. South Univ. Technol. (2008) 15: 350-355 DOI: 10.1007/s11771-008-0066-z Settlement behavior of coal mine waste in different surrounding rock conditions MA Chun-de(马春德)1, LI Xi-bing(李夕兵...; Abstract: In order to investigate the influence of complex conditions of in-situ surrounding rocks on the settlement behavior of nubbly coal mine waste subjected to high gravity pressure......