共搜索到7476条信息,每页显示10条信息,共748页。用时:0小时0分0秒488毫秒
Effect of substrate temperature on microstructures and dielectric properties of compositionally graded BST thin films ZHANG Bai-shun(张柏顺), GUO Tao(郭 涛), ZHANG Tian-jin(章天金), WANG Jin-zhao(王... (BST) (x = 0-0.3) thin films were prepared on Pt/Ti/SiO2/Si substrate at different substrate temperatures ranging from 550 ℃ to 650 ℃ by radio-frequency (rf) magnetron sputtering. The effect......
Preparation and Properties of Amorphous NiFe/Cu/NiFe Thin Films JIANG Ya-dong1,YE Yun1,ZENG Hong-juan1,HU Wen-cheng2 (1.School of Optoelectronic Information, University of Electronic Science.... Furthermore, the GMI value of NiFe/Cu/NiFe amorphous thin film with a sandwich structure is higher than that of single-layer ferromagnetic films of the same thickness. 关键词:electroplating; permalloy......
Effect of sputtering pressure and rapid thermal annealing on optical properties of Ta2O5 thin films ZHOU Ji-cheng(周继承), LUO Di-tian(罗迪恬), LI You-zhen(李幼真), LIU Zheng(刘 正) School of Physics...; Abstract: Ta2O5 thin films were deposited by DC reactive magnetron sputtering followed by rapid thermal......
Electrochemically switched ion exchange performances of capillary deposited nickel hexacyanoferrate thin films HAO Xiao-gang(郝晓刚), GUO Jin-xia(郭金霞), LIU Shi-bin(刘世斌), SUN Yan-ping(孙彦平) Department...; Abstract: Thin films of capillary deposited nickel hexacyanoferrate(NiHCF) were......
Effect of crystallization temperature on microstructure and ferroelectric property of Bi3.25Eu0.75Ti3O12 thin films prepared by MOD method HE Lin(何 林)1,2, ZHANG Tong(张 彤)3, TANG Ming-hua(唐明华)1,2... Abstract: Europium-substituted bismuth titanate (Bi3.25Eu0.75Ti3O12) thin films were deposited on the Pt/Ti/SiO2/Si(111) substrates by metal-organic decomposition (MOD) method using a repeated......
Effects of annealing temperature on microstructure and ferroelectric properties of Bi0.5(Na0.85K0.15)0.5TiO3 thin films GONG Yue-qiu(龚跃球)1, ZHENG Xue-jun(郑学军)1, 2, GONG Lun-jun(龚伦军)1, MA Yin(马 颖)1... (BNKT15) thin films were synthesized by metal-organic decomposition (MOD) at annealing temperatures of 650, 680, 710 and 740 °C, and the effects of annealing temperature on the microstructure......
" name="ChDivSummary"><正> Excellent epitaxial growth of supercon-ducting YBa2 Cu3 O7-x thin films have beenrealized on(100)SrTiO3 and(100)ZrO2substrates by a planar rf or DC-magnetronsputtering...High Jc Epitaxial Superconducting YBa2Cu3O7-x Thin FilmsChen Lanfeng Zhou Li Wang Chaoqun General Research Institute of Non-ferrous Metals.Beijing,China Li Lin Zhao Bairu Zhang Yinzi Qiu Xianggang......
Deformation Strength of Nanocrystalline Thin FilmsW.Blum1,P.Eisenlohr21. Department of Materials Science, Inst.I, University of Erlangen-Nürnberg2. Department of Chemical Engineering and Materials Science, Michigan State University摘 要:The data of deformation strength and microstructure of thin films of nanocrystalline Pd recently provided by Colla et al......
Preparation and oxygen-sensing properties of TiO2 porous thin films on alumina substrate LI Ming-li(李明利),XU Ming-xia(徐明霞), LI Yan(李 岩) School of Materials Science and Engineering, Key Laboratory...-temperature properties of porous films are not notably improved with the increasing of the content of PEG. Key words: TiO2 porous thin film; organic template; sol-gel method; oxygen-sensitivity 1......
) Abstract:The effect of annealing treatment on the structure of CdS films was investigated.The cadmium sulfide thin films were prepared by chemical bath deposition, and were annealed at nitrogen atmosphere... surface. It was found that thermal annealing could produce large grains of CdS thin films, remove the air contamination and reduce the oxygen content on the CdS films surface. Therefore,the CdS films......