Microstructure and wear resistance of Ti-3Zr-2Sn-3Mo-15Nb (TLM) alloy YU Zhen-tao(于振涛)1, ZHENG Yu-feng(郑玉峰)2, NIU Jin-long(牛金龙)1, HUANGFU Qiang(皇甫强)1, ZHANG Ya-feng(张亚峰)1, YU Sen(余森)1 1...: The effects of heat treatment on the microstructure and phase constitution of Ti-3Zr-2Sn-3Mo-15Nb (TLM) alloy were investigated by optical microscopy, X-ray diffractometry and transmission electron......
......
decreases for all the deformed AZ80 alloys and increases for the as-cast alloy. MATHIEU et al[10] also proved that corrosion rate is variable based on the investigation of AZ91D. With increase of time... of corrosion resistance of AZ80 alloys, because α-Mg is protected under the coverage of continuously distributed β particles. 2) AZ80 alloy deformed at 250 ?C with the deformation of 83% has the best......
, STORMER M, DIETZEL W, MANDL S. Deposition and properties of novel microcrystalline Mg alloy coatings [J]. Surf Eng, 2007, 23(5): 339-343. [8] ANGELINI E, GRASSINI S, ROSALBINO F, FRACASSIF, D’AGOSTINOR. Electrochemical impedance spectroscopy evaluation of the corrosion behavior of Mg alloy coated with PECVD organosilicon thin film [J]. Prog Org Coat, 2003, 46(2): 107-111. [9] TIAN X B, WEI CB, YANG S......
......
of AZ31B Mg alloy tube for warm tube hydroforming [C]//KIM D W. Proceedings of the 9th International Conference on Technology of Plasticity. Korea: KSTP, 2008: 1274-1279. [12] ESNAOLA J A, TORCA I... Wrinkling behavior of magnesium alloy tube in warm hydroforming TANG Ze-jun(汤泽军), LIU Gang(刘 钢), HE Zhu-bin(何祝斌), YUAN Shi-jian(苑世剑) School of Materials Science and Engineering, Harbin Institute......
ZK60 alloy ingot (the chemical composition (mass fraction, %): Zn 5.6, Zr 0.54, Fe≤0.003, Ni≤0.002, Mg balance) with a diameter of d129 mm was used in the experiments. The specimens were taken from... temperature range might be ignored during fast cooling. However as reported by WEI et al[18], Mg7Zn3 phase may form in Mg-Zn binary system in which Zn content is increased. 4.2 Formation of MgZn2......
]XUE Wen-bin, DENG Zhi-wei, CHEN Ru-yi, et al. Growth regularity of ceramic coatings formed by microarc oxidation on Al-Cu-Mg alloy[J]. Thin Solid Films, 2001, 372: 114-117. [7]TIAN Jun, LUO Zhuang-zi... of Mechanics, Chinese Academy of Sciences, Beijing 100080, China) Abstract: Amorphous [Al-Si-O] coatings were deposited on aluminum alloy by plasma electrolytic oxidation(PEO). The process parameters......
of the structural aircraft parts. 2 EXPERIMENTAL The Al alloy assessed in this investigation was AA 7010-T7651 with a chemical composition of Zn 6.30, Mg 2.34, Cu 1.75, Zr 0.12, Fe 0.05, Si 0.04, Ti..., Mn or Si in solid solution in Al alloys would result in an increase in resistivity of 0.094, 0.344, 0.54, 1.74, 2.56, 2.88, 2.94 or 1.02μΩ·cm, respectively. The measured concentrations of Zn, Cu, Mg......
......