共搜索到23276条信息,每页显示10条信息,共2328页。用时:0小时0分0秒248毫秒
The Technological Improvements of Aluminum Alloy Coloring by Electrolysis LI Nai-jun1 (1.Teachers College, Shenyang University, Shenyang 110015, P. R. China) 摘要:The technological process of coloring golden-tawny on aluminum alloy by electrolysis was improved in this paper. The optimum composition of electrolyte was found, the conditions of deposition and anodic oxidation by electrolysis were......
Microstructure and Performances of Nanocrystalline Zinc-nickel Alloy Coatings LI Guang-yu1,NIU Li-yuan1,JIANG Zhong-hao1,LIAN Jian-she1 (1.The Key Lab of Automobile Materials, Ministry of Education, China, College of Materials Science and Engineering, Jilin University, Nanling Campus, Changchun, 130025, China) 摘要:Nanocrystalline zinc-nickel alloy coatings were deposited from an alkaline......
Alloy 20不锈钢薄板等离子弧焊接工艺研究赵斌,王宾宾,王小华中国船舶重工集团公司第七二五研究所摘 要:对Alloy 20不锈钢薄板进行了等离子弧焊接工艺试验研究.结果表明,采用等离子弧焊接方法,ERCr Ni Mo-3焊材及合理的焊接工艺参数,等离子弧焊接工艺可用于Alloy 20不锈钢薄板的焊接,焊接接头各项性能均能满足要求.关键词:Alloy 20;不锈钢薄板;等离子弧焊接;......
)Abstract:Stainless die with micro-groove and micro-hole have been designed and manufactured, which has been used to study superplastic microforming of 2091Al-Li alloy by means of superplastic forming... micro-rib specimen, behavior of material could be understood well.Key words:superplasticity; microforming; extrusion; 2091Al-Li alloy......
%,预还原温度为1 150 ℃,预还原时间为30 min,电炉熔分温度为1 450 ℃,熔分时间为15 min的条件下,经转底炉预还 原-电炉熔分后,获得镍质量分数为8.68%,镍回收率97.62%,铁质量分数为86.23%的镍铁合金,该合金可用作不锈钢生产原料.关键词:红土镍矿;预还原;电炉熔分;镍铁合金Production of Ni-Fe alloy from... of Precious Metals, State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming 650106, China)Abstract:The production of Ni-Fe alloy from nickeliferous......
Trans. Nonferrous Met. Soc. China 22(2012) s656-s660 Microforming of superplastic 5083 aluminum alloy Md. Abu Mowazzem HOSSAIN1, Sung-Tae HONG1, Kyu-Yeol PARK1, Young-Sang NA2 1. School of Mechanical...: The mechanical behavior of superplastic 5083 aluminum alloy during microforming process was investigated by finite element analysis. A micro V-groove die was modeled to analyze the effects of forming......
纳米SiC颗粒强化AA6061的磨粒磨损行为李晓丹,翟玉春,马军平东北大学材料与冶金学院摘 要:实验制备了纳米SiC颗粒强化AA6061基材料,并考察了其微观组织,硬度及磨损性能.结果表明:在20 N载荷下,强化试样的磨损率及摩擦系数均低于AA6061基体,其中0.6%SiC/AA6061复合材料的磨损率较基体降低50%.这主要是由于SiC颗粒自身良好的载荷承载能力,加之增强颗粒/基体间界面良好的结合,使SiC颗粒的添加提高了复合材料的磨损抗力.同时,促进了富铁机械转移层的形成,降低了摩擦系数和磨损率.AA6061基体和强化材料在20 N载荷下的磨损机制均为磨粒磨损.关键词:干滑动磨损;AA6061;纳米SiC强化;磨粒磨损;......
Study on Thermomagnetic Treatment Fe-25.5Cr-12Co Permanent Magnetic Alloy Zhen Liang1,GAO Run-sheng2,ZHU Dan-yang1,SUN Xue-yin1,SHAO Wen-zhu1,XU Ren-gen1 (1.Technology and Development Centre... Fe-25.5Cr-12Co alloy by different process of thermomagnetic treatment were investigated. It is found that magnetic properties are sensitive to parameters of thermomagnetic treatment process in magnetic......
荧光分析法检测Cl-溶液中AA6061铝合金的腐蚀夏铁锋1,李光勇2,李康1,高立新1,张大全11. 上海电力学院环境与化学工程学院2. 河南省医药技师学院制药工程系摘 要:采用荧光分析法和失重法研究了AA6061铝合金在不同Cl-浓度溶液中的腐蚀行为.结果表明,荧光分析法能够很好地监测铝合金的腐蚀过程,与失重法所得结果的趋势具有一致性.在含有不同Cl-浓度的溶液中,AA6061铝合金在浸泡初期,腐蚀反应速率较快;随着浸泡时间的延长,腐蚀反应速率逐渐降低.关键词:铝合金;荧光;Cl-溶液;腐蚀;......
J. Cent. South Univ. (2018) 25: 1573-1581 DOI: https://doi.org/10.1007/s11771-018-3849-x Derivation and application of concentration formula of alloy genes of DO3-type in BCC alloy systems PENG... and Engineering, Central South University, Changsha 410083, China Central South University Press and Springer-Verlag GmbH Germany, part of Springer Nature 2018 Abstract: Taking Ta–W alloy system......