共搜索到6961条信息,每页显示10条信息,共697页。用时:0小时0分0秒640毫秒
Trans. Nonferrous Met. Soc. China 27(2017) 2381-2389 Effects of solid solution treatment and cooling on morphology of LPSO phase and precipitation hardening behavior of Mg-Dy-Ni alloy Li-tao YUAN1...: Effects of solid solution treatment and cooling on the morphology of long period stacking order (LPSO) phase and precipitation hardening behavior of Mg-2Dy-0.5Ni (molar fraction, %) alloy were......
Age Hardening of Rapidly-Solidified Mo-Th-B AlloysNing Yuantao Institute of Precious Metals,Kunming,China摘 要:<正> The splat foils with 30~35 μm... hardening response,especially for Mo-8Th-0.8B alloy.The precipitates associated with agehardening were identified to be ThB4(Tetragon) and Mo2B(C16,BTC).The times of reaching age hardening peak forboth......
......
Trans. Nonferrous Met. Soc. China 23(2013) 1595-1601 Extrusion and precipitation hardening behavior of AZ91 magnesium alloy M. THIRUMURUGAN, S. KUMARAN Department of Metallurgical and Materials... °C, respectively with extrusion ratio of 4:1 followed by precipitation hardening treatment (T6). The coarse and segregated Mg17Al12 intermetallic precipitate in AZ91 magnesium alloy was refined......
Trans. Nonferrous Met. Soc. China 24(2014) 2326-2330 Precipitation hardening behavior of dilute binary Al-Yb alloy Chao-lan TANG1, De-jing ZHOU2 1. College of Electromechanical Engineering, Guangdong... Abstract: The precipitation hardening behavior in dilute Al-Yb alloys upon annealing at different temperatures was investigated to shed light on the mechanism of micro-alloying element in aluminum alloys......
hardening on fracture toughness of micro-alloyed steel [J]. Journal of Materials Engineering and Performance, 2014, 23(1): 152–168. [6] HAN Y, SHI J, XU L, CAO, W Q, DONG H. TiC precipitation induced...J. Cent. South Univ. (2017) 24: 2767-2772 DOI: https://doi.org/10.1007/s11771-017-3690-7 Precipitation behavior of Ti in high strength steels WU Si-wei(吴思炜), LIU Zhen-yu(刘振宇), ZHOU Xiao-guang(周晓光......
-silicon-copper alloys are enhanced through precipitation hardening. The response of these alloys to age-hardening is very slow. To overcome this problem, 0.2, 0.4 and 0.7 wt.% magnesium were added to Al-10.5Si-3.4Cu alloy. The new alloys were subjected to two types of precipitation hardening processes different in the solutionizing stage. The results showed that the presence of various amounts......
Secondary hardening behavior of 15CrMnMoV thin rolled tubeCi DING and Weixin HAN Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China摘 要:15CrMnMoV rolled tube is applied to many critical parts of helicopter. The secondary hardening behavior of the steel which varied with the treating process is essential for further usage......
and large forging is caused by the secondary phase precipitation from the transformed β above 830 ℃. The precipitation strengthening effect on the little bar is smaller than that of the large forging because of the recrystallization softening effect. Key words: TA15 titanium alloy; heat treatment; deformation degree; recrystallization; precipitation hardening TA15钛合金具有中等的室温强度,优良的高温性能和焊接性能,并可制成各种半成品,如棒材......
and distribution, a calculation based on Orowan mechanism shows that the precipitation hardening offers 166 MPa yielding strength increase. The precipitation sequence is as follows: TiN, TiC, NbC, NbN. Key words: DH36; carbides; carbonitrides; precipitation hardening; precipitation thermodynamic DH36级船板钢属于高强度船体结构用钢,具有强度高,低温冲击韧性佳,焊接性能良好等特点,在造船工业中应用广泛[1-2].目前,国内外工业级高强度船板钢普遍采用控轧控冷和微合金化有机结合的方法细化铁素体晶粒并析出第二相粒子,以提高其力......