MPa, 886 MPa, 22.83% and 24.37%, respectively. The tungsten alloy is simply made up of body centered cubic tungsten phase and face centered cubic Fe3Ni2 solid solution phase. With the increase of sintering temperature, the fracture morphology of tungsten alloy is transformed from intergranular brittle fracture to transgranular brittle fracture, dimple ductile fracture, bonding phase tearing......
pattern. Fig.2(c) shows the fracture characteristics of the as-cast Mg97Zn1Y2 alloy, which can be described as a brittle quasi-cleavage mode including mainly cleavage planes from 2H-Mg phase and inter... Tensile fracture of as-cast and hot rolled Mg-Zn-Y alloy with long-period stacking phase WANG Bai-shu(王柏树)1, 2, XIONG Shou-mei(熊守美)1, LIU Yong-bing(刘勇兵)3 1. State Key Laboratory of Automotive......
Factors Influencing High Temperature Thermo Plasticity of BNbRE Steel at the Third Brittle Zone Chen Lin1,Liu Yuyan1,Zong Wei1,Tian Zhongliang1,Ren Huiping1,Gao Michao1,Bao Xirong1 (1.Material... in the practiced production, the effect of two factors, i. e. deformation temperature, deformation velocity, on thermo plasticity of BNbRE steel at the third brittle zone was quantitatively......
......
precipitated from austenite phase during cooling. The Cu rich chem-ical compounds are brittle substance such as Cu2S, Cu2O and ε-Cu etc. Key words:304HC stainless steel; hot ductility; brittle compounds......
;断裂机理 中图分类号:TU 452 文献标识码:A Plane shear (ModeⅡ) fracture experiment analysis of brittle rock at high temperature XIE Hai-feng, RAO Qiu-hua...) tests were used to study the shear fracture characteristics and mechanism of brittle rock at high temperature. The physical and mechanical properties of brittle rock at high temperature were......
Mechanical behavior and failure analysis of brittle sandstone specimens containing combined flaws under uniaxial compressionYANG Sheng-qi(杨圣奇)1, 2, JING Hong-wen(靖洪文)1, XU Tao(徐涛)3(1. State Key... are obtained by the acoustic emission, which can be used to monitor the crack initiation and propagation. The ultimate failure mode and crack coalescence behavior are evaluated for brittle sandstone specimens......
Macro-microscopic morphology and phase analysis of TiAl-based alloys sheet fabricated by EB-PVD method ZHANG De-ming(章德铭)1, CHEN Gui-qing(陈贵清)1, HAN Jie-cai(韩杰才)1, ZHANG Xing-hong(张幸红)1, YAO... was fabricated successfully by using electron beam-physical vapor deposition(EB-PVD) method. The microscopic morphology and phase composition of specimens in various states were analyzed by atomic......
......
Effect of ball milling time on microstructure and properties of Laves phase NbCr2 alloys synthesized by hot pressing XIAO Xuan(肖 璇)1, 2, LU Shi-qiang(鲁世强)1, HU Ping(胡 平)1, HUANG Ming-gang(黄铭刚)1...; Abstract: Laves phase NbCr2 alloys with a composition of Nb-66.7Cr (molar fraction, %) were prepared by mechanical alloying and hot pressing. The microstructures and properties of the Laves phase NbCr2......