共搜索到3505条信息,每页显示10条信息,共351页。用时:0小时0分0秒368毫秒
Effects of increase extent of voltage on wear and corrosion resistance of micro-arc oxidation coatings on AZ91D alloy L? Wei-ling(吕维玲)1, CHEN Ti-jun(陈体军)1, MA Ying(马 颖)1, XU Wei-jun(徐卫军)1, 2...; Abstract: The effects of increase extent of voltage on the wear resistance and corrosion resistance of micro-arc......
......
On the Friction and Wear Behaviors of Dental Machinable Porcelain YU Hai-yang1,ZHOU Zhong-rong1,CAI Zhen-Bing1 (1.Tribology Research Institute, Southwest Jiaotong University, Chengdu, China... machinable porcelain are essential. The friction and wear behavior of new generation industrially prefabricated Cerec Vitablocs Mark Ⅱ against uniform Si3N4 ball has been performed using a small amplitude......
Friction and Wear Characteristics of Mg-Al Alloy Containing Rare Earths 杨晓红1,刘勇兵1,祁庆琚1 (1.College of Materials Science and Engineering, Jilin University, Changchun 130025, China) Abstract:The influence of rare earth on the friction and wear characteristics of magnesium alloy AZ91 and AM60 were studied. The results show that the wear resistance properties of rare earth magnesium alloys......
Improving wear resistance of magnesium alloy AZ91D by TiN-CrN multilayer coating MIAO Qiang(缪 强)1, 2, CUI Cai-e(崔彩娥)1, PAN Jun-de (潘俊德)1, ZHANG Ping-ze(张平则)2 1. Research Institute of Surface... on the surface of magnesium alloy AZ91D to improve its wear resistance. The wear behavior was investigated by test of ball on disc sliding. The composition and microstructure of the coating were also analyzed......
......
Effect of Cooling Rate after hot Deformation on Structure and Mechanical Properties of Low Alloy Wear Resistance Cast iron Liu Jianping1,Li Lixia2 (1.College of Environmental & Chemical Engineering... of cooling rate after 40% hot deformation on structure and mechanical properties of low alloy wear resistance cast iron was investigated by metallographic, scanning electron microscopes and detection......
......
Study on the Thermal Fatigue Behavior of Hot Deformed Wear Resistance Cast Iron and Effect of Carbide Dong Litao1,Li Xingyuan2,Liu Rongchang1,Chen Xiuhong1 (1.Department of Mechanics... behavior of wear resistance cast iron with different quantity of deformation has been investigated. The results show that eutectic carbide is the main location and passage for initiation and extension......
Slurry wear characteristics of zinc-based alloys: Effects of sand content of slurry, silicon addition to alloy system and traversal distance  ... with the observations pertaining to the effects of specimen and slurry compositions as well as traversal distance on the slurry wear response of a zinc-based alloy. The composition of the alloy was altered......