Article ID: 1003-6326(2005)02-0375-04 Interface evolution of TiAl/Ti6242 transient liquid phase joint using Ti, Cu foils as insert metals DUAN Hui-ping(段辉平)1, K. H. Bohm2, V. Ventzke2, (1... D-21502, Germany) Abstract: The interface evolution of TiAl/Ti6242 joint produced by transient liquid phase(TLP) bonding with Ti, Cu foils as insert metals was investigated. The results show......
......
Transient Liquid Phase Bonding of IN738LC/MBF-15/IN738LC:Solidification Behavior and Mechanical PropertiesB.Binesh,A.Jazayeri Gharehbagh摘 要:Transient liquid phase(TLP) bonding of IN738 LC superalloy was carried out using a rapidly solidified MBF-15 Ni-based foil. The effects of bonding temperature(1130–1170 °C) and time(5–120 min) as well as foil......
Effects of Silicon Nanoparticles on the Transient Liquid Phase Bonding of 304 Stainless SteelH.M.Hdz-García1,A.I.Martinez2,R.Mu?oz-Arroyo1,J.L.Acevedo-Dávila1,F.García-Vázquez1,F.A.Reyes-Valdes1摘 要:Transient liquid phase(TLP) bonding of 304 stainless steel with nickel based filler metal, BNi-9, was performed to study the influence of silicon......
Ultrasound-Assisted Transient Liquid Phase Bonding of Magnesium Alloy Using Brass Interlayer in AirZhiwei Lai1,2,3,4,Ruishan Xie2,5,Chuan Pan3,Xiaoguang Chen2,Lei Liu2,Wenxian Wang5,Guisheng Zou21... id="ChDivSummary" name="ChDivSummary">The microstructure evolution and oxide film behavior in ultrasound-assisted transient liquid phase(U-TLP) bonding of Mg alloy were investigated by applying......
......
......
......
liquid, the water occupies the pores. While in case of unsaturated soil, as pore water and pore air coexist in the pores, the seepage process is generally a two-phase flow problem with different flow...J. Cent. South Univ. (2017) 24: 1866-1880 DOI: https://doi.org/10.1007/s11771-017-3594-6 Forming condition of transient saturated zone and its distribution in residual slope under rainfall......