INDUCTION PLASMA REACTIVE DEPOSITION OF TUNGSTENCARBIDE FROM TUNGSTEN METAL POWDER M.I.Boulos1,X.L.Jiang2 (1.Department of Chemical Engineering, University of Sherbrooke, Sherbrooke, J1K 2R1... the tungsten powder and methane in the induction plasma, and the secondary carburization of the deposit on substrate at high temperature. Optical microscopy and scanning electron microscopy were used to examine......
of transient thermal shock all mainly concentrates on the shallow surface layer of tungsten(about 500 μm) under different transient heat flux(duration 0.5 ms).The results are useful for the structural design...A Simulation Study on the Thermal Shock Behavior of Tungsten Mock-Up under Steady-State Heat LoadsYanxin Wang,Shuming Wang,Qing Ye,Qingzhi Yan,Changchun GeDepartment of Materials Science......
......
......
......
......