共搜索到20739条信息,每页显示10条信息,共2074页。用时:0小时0分0秒412毫秒
Burning products of TA15 titanium alloy by friction oxygen concentration methodNan Sui,Guang-Bao Mi,Meng-Qi Yan,Jing-Xia Cao,Xu HuangAviation Key Laboratory of Science and Technology on Advanced... mechanism of the burning products of TA15 titanium alloy were investigated by friction oxygen concentration method, associated with in situ observation, X-ray diffraction(XRD),scanning electron......
Effect of CaO composition on oxidation and burning behaviors of AM50 Mg alloy Jin-Kyu LEE, Shae K. KIM Advanced Material Division, Korea Institute of Industrial Technology, 7-47... into AM50 Mg alloys. Key words: Mg alloy; CaO; oxidation behavior; burning behavior 1 Introduction AM50 Mg alloy has already been applied to certain automobile parts, such as instrument panel, seat......
features of the true stress-true strain curves can be explained based on deformation mechanism analysis. Key words: AZ31 magnesium alloy; twinning; basal slip, non basal slip  ...%, 4% and 6%) were obtained by using titanium alloy stopper ring of different heights under dynamic compressive loading. The inner diameter of the stopper ring is 7.5 mm and its outer diameter is 14.5 mm......
Plasma surface alloying of titanium alloy for enhancing burn-resistant property ZHANG Ping-ze(张平则) 1, XU Zhong(徐 重) 1,2, ZHANG Gao-hui(张高会) 2, HE Zhi-yong(贺志勇) 2,YAO Zheng-jun(姚正军) 1 1.School... 030024,China Received 28 July 2006; accepted 15 September 2006 Abstract: Conventional titanium alloy may be ignited and burnt under high temperature, high pressure and high gas flow velocity condition......
The Progress on Laser Surface Modification Techniques of Titanium Alloy Al Ding-fei1,LIANG Cheng2,XIA Chun-huai2,SONG Yan2,PAN Lin2,TAO Xi-qi2 (1.School of Physical Science and Technology Wuhan University, Wuhan 430070,P. R China;2.Wuhan Research Institute of Materials Protection, Wuhan ,430030, P. R China) 摘要:Titanium alloy is widely used in aviation, national defence, automobile, medicine......
......
Deformation behavior of TC1 titanium alloy sheet under double-sided pressure WANG Zhong-jin(王忠金), SONG Hui(宋 辉),WANG Zhe(王 哲) School of Materials Science and Engineering, Harbin Institute... bulge(VPB) tests of an annealed TC1 titanium alloy sheet were carried out under two different conditions: double-sided pressure bulging and conventional single-sided pressure bulging. The automated......
)Abstract:A new cup-drawing process of BT20 titanium alloy was studied. Tensile tests were carried out at room temperature, and then cup-drawing experiments were carried out with conical female die at high temperatures. The results show that the plasticity of BT20 titanium alloy is bad, σs/σb is big, n is small, so it is not suitable for BT20 titanium alloy which draws at room temperature, even......
Modeling corrosion behavior of gas tungsten arc welded titanium alloy M. Balasubramanian1, V. Jayabalan2, V. Balasubramanian3 1. Department of Mechanical Engineering, Maamallan Institute... alloy in marine environment were explained. Besides the rapid advance of titanium metallurgy, this is also due to the successful solution of problems associated with the development of titanium alloy......
......