共搜索到8975条信息,每页显示10条信息,共898页。用时:0小时0分0秒386毫秒
......
Research of Tribological Behaviors of a New Aluminum Bronze WANG Zhi-ping1,XU Jian-lin1,CHEN Chao2 (1.State Key Lab of Gansu New Non-ferrous Metal Materials, Lanzhou University of Science... strength and wear resistant aluminum bronze, with its friction coefficient and wear-rate lower than those of ZQAl9-4 and ZQAl10-4-4 alloys in terms of Chinese national standard.The results showed......
High temperature performance of arc-sprayed aluminum bronze coatings for steel ZHANG Zhong-li(张忠礼)1, LI De-yuan(李德元)1, WANG Shui-yong(王水勇)2 1. School of Materials Science and Engineering... April 2006 Abstract: The high-temperature oxidation behavior of arc-sprayed aluminum bronze coatings on steel substrate was studied during isothermal exposures in air at 900 ℃. The surface......
......
......
Preparation, mechanical properties and wear behaviors of novel aluminum bronze for dies LI Wen-sheng(李文生)1, WANG Zhi-ping(王智平)1, LU Yang(路 阳)1, GAO Yong(高 勇)2, XU Jian-lin(徐建林)1 1. State Key...; Abstract: A modified single melt technique involving joint charging was developed for preparation of aluminum bronze, Cu-14%Al-X(mass......
during the turning of aluminum bronze using high-speed steel and cemented carbide tools have been studied. The tool wear samples were prepared by using M2 high-speed steel and YW1 cemented carbide tools to turn a novel high strength, wear-resistance aluminum bronze without coolant and lubricant. Adhesion of workpiece materials was found on all tools’ surface. The diffusion couples made of tool......
Effect of Deformation on Phase Transformation of α+γ2→β in Aluminum Bronze宋伟,杨景茹,阎丽娟摘 要:The phase transformation kinetics of α+γ2→β in aluminum bronze under different condition were studied by DSC, and the effect of deformation on the phase transformation of α+γ2→β in aluminum bronze was discussed. The results show that the transformation temperature......
......
behavior of a hotextruded nickel aluminum bronze was studied.Three kinds of samples subjected to the hot-extrusion,annealing and quenching conditions were prepared and immersion tests in 3.5% NaCl solution...Effect of microstructure on the mechanical and corrosion behaviors of a hot-extruded nickel aluminum bronzeDatong ZHANG,Ruiping CHEN,Weiwen ZHANG,Zongqiang LUO and Yuanyuan LI School of Mechanical......