共搜索到2350条信息,每页显示10条信息,共235页。用时:0小时0分0秒421毫秒
Extrusion process of lead-clad glass fiber compositesSUN Hong-fei(孙宏飞), FANG Wen-bin(房文斌),HAN Fei(韩 飞),HE Wen-xiong(贺文雄),WANG Er-de(王尔德)(School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China)Abstract:The extrusion process of lead-clad glass fiber composites was studied. Lead-clad glass fiber composites with diameter ranging in 0.5-1.0mm were......
......
Effect of extrusion wheel angular velocity on continuous extrusion forming process of copper concave bus bar WU Peng-yue(吴朋越)1, XIE Shui-sheng(谢水生)1, LI Hua-qing(李华清)1, YAN Ming(鄢 明)1, HUANG...; Abstract: The continuous extrusion forming process for producing large section copper concave bus bar under different extrusion wheel......
Effect of extrusion ratio on coating extrusion of Pb-GF composite wire by numerical simulation and experimental investigation WANG Xin(王 欣), SUN Hong-fei(孙宏飞), FANG Wen-bin(房文斌) School...; Abstract: The extrusion ratio is one of the key parameters for manufacturing......
Microstructure and corrosion behavior of Mg-Sn-Ca alloys after extrusion T. ABU LEIL1, N. HORT1, W. DIETZEL1, C. BLAWERT1, Y. HUANG1, K. U. KAINER1, K. P. RAO2 1. GKSS... and potentio-dynamic measurements. The results obtained on the alloys Mg-3Sn (T3), Mg-3Sn-1Ca (TX31), and Mg-3Sn-2Ca (TX32) indicate the presence of the same phases in as-cast and after extrusion, namely......
......
and Joining (Harbin Institute of Technology), Harbin 150001, China; 2. Zhejiang Yinlun Machinery Company Limited, Tiantai 317200, China)Abstract:A new method named rotating extrusion was developed to mitigate residual distortion of thin-plate weldments. the basic principle and characteristic of rotating extrusion as well as an efficient rotating extrusion device were introduced. Systematic......
Effects of extrusion deformation on mechanical properties of sub-micron Si3N4p/2024 composite XIU Zi-yang(修子扬)1, CHEN Guo-qin(陈国钦)2, LIU Yan-mei(刘艳梅)2, YANG Wen-shu(杨文澍)2, WU Gao-hui(武...; Abstract: Si3N4p/2024Al composite was fabricated by squeeze casting method and treated by extrusion deformation. Microstructure analyses indicate......
......
......