共搜索到10114条信息,每页显示10条信息,共1012页。用时:0小时0分0秒516毫秒
......
......
Effect of extrusion ratio on coating extrusion of Pb-GF composite wire by numerical simulation and experimental investigation WANG Xin(王 欣), SUN Hong-fei(孙宏飞), FANG Wen-bin(房文斌) School... the lead-glass fiber (Pb-GF) composite wire by coating extrusion. The effect of extrusion ratio on coating extrusion of Pb-GF composite wire was studied by finite element numerical simulation......
THE PHYSICAL SIMULATION ON EXTRUSION PROCESS OF GLASS FIBER COMPOSITE WIRE COATED BY LEAD F.Han1,H.F.Sun1,W.B.Fang1,W.X.He1,E.D.Wang1 (1.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China) Abstract:The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from......
. Production of stainless steel wire-reinforced aluminium composite sheet by explosive compaction [J], Journal of Materials Science, 1977, 12(3): 522–530. [4] SARAVANAN S, RAGHUKANDAN K. Diffusion kinetics..., 2016, 16(4): 563–568. [11] GULENC B, KAYA Y, DURGUTLU A, GULENC I T, YILDIRIM M S, KAHRAMAN N. Production of wire reinforced composite materials through explosive welding [J]. Archives of Civil......
during wet wire drawing and that precision wire products are affected by the heat generated in the contact zone [7]. DENG et al [8] performed wire-drawing tests with a ceramic composite die and 65-Mn... Trans. Nonferrous Met. Soc. China 22(2012) 1723-1731 Advanced simulation of die wear caused by wire vibrations during wire-drawing process LEE Kyung-Hun1, LEE Sang-Kon2, KIM Byung-Min3 1. Precision......
. The ceramic composite wire drawing die was prepared by hot pressing sintering, the sintering temperature was 1 700- 1 800 ℃, the pressure was 30 MPa, the heat preservation was 10-30 min... 1. Table 1 Mechanical properties of TiC/Al2O3 ceramic composite specimen 2.3 Lubrication and wear testing The drawn wire is 65 Mn steel; its diameter is 4.5 mm, which changed to 4 mm after......
......
. The developmental trends of the preparation of fixed diamond wire saw were proposed. Key words:diamond; wire saw; fixed grits; cladding; composite electroplating; depositional mechanism 随着光电产业和半导体产业的快速发展,单晶硅片和蓝宝石等贵重...未达到统一,应明确复合电沉积机理. REFERENCES [1] 刘绪鹏. 金刚石线锯的复合电镀法制备及其性能研究[D]. 大连: 大连理工大学, 2008. LIU Xu-peng. Study on the composite plating manufacturing and the performance of fixed diamond wire[D]. Dalian: Dalian......
inhibited and the wettability of molten pool is improved by adding Ti-Si-Mg-Al flux-cored wires. With 15Ti-5Si-5Mg-Al flux-cored wire as filled composite, the maximum tensile strength of the welded joint... Trans. Nonferrous Met. Soc. China 22(2012) 305-311 Effect of Ti-Si-Mg-Al wire on microstructure and mechanical properties of plasma arc in-situ welded joint of SiCp/Al composites LEI Yu-cheng1, 2......