Study on Dry Friction and Wear Properties of TiAl Alloy

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2009年第S1期

论文作者:耿明 孙东立

文章页码:179 - 182

摘    要:A Ti-50Al alloy has been prepared by vacuum pressure casting.The full lamellar microstructure (FL) has been formed upon heat treating at 1400 ℃ and then furnace cooling.The frictional wear behavior of the alloy at the room temperature has been tested and its wear mechanism has been studied.The results show that with the increase of the load and sliding speed,the wear rate of the as-cast Ti-50Al alloy rises and the friction coefficient declines.When sliding speed is lower than 1.0 m/s the wear rate of the FL Ti-50Al alloy increased with the load and sliding speed,but the friction coefficient is relatively invariable at about 0.5.The wear mechanism is mainly of abrasive wear and adhesive wear.When sliding speed is higher than 1.5 m/s,the wear mechanism has changed to mainly oxidization wear so that the wear rate of the FL Ti-50Al alloy declines significantly and the friction coefficient increases.Compared to the as-cast alloy,the FL Ti-50Al alloy has better wear resistance.

详情信息展示

Study on Dry Friction and Wear Properties of TiAl Alloy

耿明,孙东立

School of Materials Science and Engineering,Harbin Institute of Technology

摘 要:A Ti-50Al alloy has been prepared by vacuum pressure casting.The full lamellar microstructure (FL) has been formed upon heat treating at 1400 ℃ and then furnace cooling.The frictional wear behavior of the alloy at the room temperature has been tested and its wear mechanism has been studied.The results show that with the increase of the load and sliding speed,the wear rate of the as-cast Ti-50Al alloy rises and the friction coefficient declines.When sliding speed is lower than 1.0 m/s the wear rate of the FL Ti-50Al alloy increased with the load and sliding speed,but the friction coefficient is relatively invariable at about 0.5.The wear mechanism is mainly of abrasive wear and adhesive wear.When sliding speed is higher than 1.5 m/s,the wear mechanism has changed to mainly oxidization wear so that the wear rate of the FL Ti-50Al alloy declines significantly and the friction coefficient increases.Compared to the as-cast alloy,the FL Ti-50Al alloy has better wear resistance.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号