Synthetic Effects of Frequency and Duty Ratio on Growth Characteristics, Energy Consumption and Corrosion Properties of Microarc Oxidized Coating Formed on Ti6Al4V

来源期刊:Acta Metallurgica Sinica2018年第10期

论文作者:Tong Zhou Zhen-Bo Qin Qin Luo Qi Zhang Bin Shen Wen-Bin Hu Lei Liu

文章页码:1109 - 1120

摘    要:The synthetic effects of frequency and duty ratio on growth characteristics and corrosion properties of coating on Ti6 Al4 V fabricated by microarc oxidation are investigated comprehensively. Under the condition of uniform cumulating time of positive impulse width, the essence of altering frequency and duty ratio to determine the formation of coating is to vary the duration and interval time of positive pulse. The growth of coating is mainly controlled by duration time of positive pulse and hardly correlated to the interval time of positive pulse, while both duration and interval time of positive pulse have few influences on the morphology and phase structures of coating. The dynamic current is related to positive impulse width and the ratio of positive pulse on-time to pulse off-time. Regardless of uniform duration or interval time of positive pulse, the energy dissipation presents a descending tendency. The relationship between energy consumption and anticorrosion performance is contradictory, and obtaining excellent corrosion resistance is bound to sacrifice lots of energy. The duty ratio and frequency can be designed purposefully to realize the optimal process.

详情信息展示

Synthetic Effects of Frequency and Duty Ratio on Growth Characteristics, Energy Consumption and Corrosion Properties of Microarc Oxidized Coating Formed on Ti6Al4V

Tong Zhou1,Zhen-Bo Qin1,Qin Luo1,Qi Zhang1,Bin Shen1,Wen-Bin Hu2,Lei Liu1,3

1. State Key Laboratory of Metal Matrix Composites, School of Material Science and Engineering, Shanghai Jiao Tong University2. School of Material Science and Engineering, Tianjin University3. Collaborative Innovation Center for Advanced Ship and Deep-Sea Exploration, Shanghai Jiao Tong University

摘 要:The synthetic effects of frequency and duty ratio on growth characteristics and corrosion properties of coating on Ti6 Al4 V fabricated by microarc oxidation are investigated comprehensively. Under the condition of uniform cumulating time of positive impulse width, the essence of altering frequency and duty ratio to determine the formation of coating is to vary the duration and interval time of positive pulse. The growth of coating is mainly controlled by duration time of positive pulse and hardly correlated to the interval time of positive pulse, while both duration and interval time of positive pulse have few influences on the morphology and phase structures of coating. The dynamic current is related to positive impulse width and the ratio of positive pulse on-time to pulse off-time. Regardless of uniform duration or interval time of positive pulse, the energy dissipation presents a descending tendency. The relationship between energy consumption and anticorrosion performance is contradictory, and obtaining excellent corrosion resistance is bound to sacrifice lots of energy. The duty ratio and frequency can be designed purposefully to realize the optimal process.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号