CuCr25W1Ni2 contact material of vacuum interrupter

来源期刊:中国有色金属学报(英文版)2001年第2期

论文作者:王江 张程煜 张晖 杨志懋 丁秉钧

文章页码:226 - 230

Key words:CuCr contact material; vacuum induction melting; dielectric strength

Abstract: CuCr25W1Ni2 alloy was prepared by means of vacuum induction melting (VIM). A series of Cu/Cr alloys with different compositions (mass fraction, 25%~75%) and Cr grain sizes (up to 150 μm) were investigated for their differences in physical properties and breakdown voltage. The influence of alloy elements and microstructure on the performance of CuCr25W1Ni2 alloy was also discussed. Experimental results show that the chromium phase is strengthened and its size is minimized by the addition of tungsten powder. After electrical breakdown, very fine tungsten particles in the melt layer form the external nuclei in the solidification process. The microstructure of surface melt layer of CuCr25W1Ni2 alloy is much flatter. It can notably improve the dielectric strength. On the other hand, the nickel can enhance the mutual solubility of copper and chromium, and the whole alloy is strengthened.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号