混合稀土碳酸盐晶型沉淀的制备

来源期刊:中国有色金属学报1998年第2期

论文作者:柳松 马荣骏

文章页码:331 - 334

关键词:混合稀土碳酸盐 晶型沉淀 晶体结构

Key words:mixed rare earth carbonates , crystalline precipitation , crystal structure

摘    要:以碳酸氢铵为沉淀剂制备了三种混合稀土碳酸盐晶型沉淀。 研究了搅拌、[NH4HCO3]/[REO] 比、 温度、 稀土配分、稀土离子浓度和晶种对沉淀过程的影响,发现前四种因素影响程度较大。 对于轻稀土型,形成晶型碳酸盐的最佳工艺条件为温度10~80 ℃, [NH4HCO3]/[REO] 比3.3~4.0,搅拌0.25~4.0 h; 对于中钇富铕型,温度20~60 ℃, [NH4HCO3]/[REO] 比3.4~3.6,搅拌1.0~3.0 h; 对于重稀土型, 温度10~70 ℃,[NH4HCO3]/[REO] 比3.4~3.8 , 搅拌0.5~3.0 h。轻稀土型和中钇富铕型的晶体结构与镧石型稀土碳酸盐相近,重稀土型则与水菱钇石型稀土碳酸盐相似。

Abstract: The crystalline precipitation of three kinds of mixed rare earth carbonates were prepared by using ammonium bicarbonate as precipitant. The influence of various parameters, such as stirring, temperature, [NH4HCO3]/[REO] ratio, the distributions of rare earth elements, rare earthion concentration and seeds were studied systematically. The first four parameters have great effects on the precipitation process. The optimal process conditions for the preparation of crystalline precipitation of rare earth carbonates have been proposed: for light rare earth type, temperature 10~80 ℃, [NH4HCO3]/[REO] 3.4~3.6, stirring time 1~3 h; for heavy rare earth type, temperature 10~70 ℃, [NH4HCO3]/[REO] 3.4~3.8, stirring time 0.5~3 h. The crystal structures of light rare earth type and medium-yttrium and rich-europium type rare earth carbonates are similar to that of lanthanite, the crystal structure of heavy rare earth type is similar to that of tengerite.

详情信息展示

 

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号