摘    要:在试验研究基础上,提出了一种提高含砷金精矿二段焙烧—氰化浸出工艺金浸出率方法。试验结果表明,含砷金精矿经一段焙烧(450~500℃)除砷后,加入一定量的添加剂SR,再进行二段焙烧(630~650℃),然后经稀硫酸除铜后进行氰化浸出,可使金的氰化浸出率提高4.65%。该方法可获得较好的经济效益和社会效益。

Abstract: Based on experimental researches,a two-stage roasting and cyanidation technique is proposed to enhance the gold leaching rate of a gold concentrate containing arsenic.After the first stage roasting(450~500 ℃) to remove arsenic,an additive SR is added before the second stage roasting(630~650 ℃),and then dilute sulphuric acid is used for copper removal,the final process is cyanidation leaching.The test results show that the leaching rate of gold increases 4.65%,and good economic and social benefits are obtained.

详情信息展示

提高含砷金精矿二段焙烧—氰化工艺金浸出率的试验研究

薛光1,王永新2,薛元昕3

(1.山东省烟台市人民武装警察部队黄金第七支队
2.河北怀来宏达矿业有限公司
3.烟台职业学院)

摘 要:在试验研究基础上,提出了一种提高含砷金精矿二段焙烧—氰化浸出工艺金浸出率方法。试验结果表明,含砷金精矿经一段焙烧(450~500℃)除砷后,加入一定量的添加剂SR,再进行二段焙烧(630~650℃),然后经稀硫酸除铜后进行氰化浸出,可使金的氰化浸出率提高4.65%。该方法可获得较好的经济效益和社会效益。

关键词:含砷金精矿; 二段焙烧; 氰化; 金; 浸出率

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号