简介概要

180t RH工艺技术优化与改进

来源期刊:钢铁2010年第8期

论文作者:段建平

文章页码:39 - 43

关键词:RH精炼; 工艺技术; 洁净钢

Key words:RH refining; process technology; cleanliness steel

摘    要:针对180 t RH精炼工艺存在的真空度低、超低碳钢处理时间长、钢中氧含量高及脱硫效率低等问题,研究并优化了RH真空脱气、脱碳升温、脱氧、脱硫等工艺,使RH工作真空度提高到100 Pa以下,超低碳钢处理时间缩短至平均36.5 min,超低碳钢钢中氧的质量分数最低为13×10-6。优化工艺降低了钢中[H]、[N]、[C]、[O]、[S]等元素的含量,提高了钢水洁净度,缩短了RH精炼时间,提高了RH精炼生产率。

Abstract: About the 180t RH refining technology,some problems are as follows,the lower working pressure and longer vacuum treatment time for ultra low carbon steel,higher oxygen content and lower desulphurization ratio.The processing parameters of vacuum degassing,decarburizaiion,deoxidizing and desulphurizaion were investigated and optimized.The vacuum working pressure is improved less than 100Pa,the treatment time of ultra low carbon steel reduces to 36.5min,and the oxygen content is less than 13×10-6.The content of , and [S] is reduced through the optimization technology of 180t RH.Meanwhile,the treatment time is shortened and cleanliness of steel is improved.The production ratio of RH refining is improved.

详情信息展示

180t RH工艺技术优化与改进

段建平1

(1.山西省太原市山西太钢不锈钢股份有限公司)

摘 要:针对180 t RH精炼工艺存在的真空度低、超低碳钢处理时间长、钢中氧含量高及脱硫效率低等问题,研究并优化了RH真空脱气、脱碳升温、脱氧、脱硫等工艺,使RH工作真空度提高到100 Pa以下,超低碳钢处理时间缩短至平均36.5 min,超低碳钢钢中氧的质量分数最低为13×10-6。优化工艺降低了钢中[H]、[N]、[C]、[O]、[S]等元素的含量,提高了钢水洁净度,缩短了RH精炼时间,提高了RH精炼生产率。

关键词:RH精炼; 工艺技术; 洁净钢

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号