焦炉煤气自重整炉气成分与温度变化规律研究

来源期刊:钢铁2009年第4期

论文作者:曹朝真 郭培民 赵沛 庞建明

文章页码:11 - 15

关键词:焦炉煤气; 自重整; 直接还原铁

Key words:coke oven gas; self-reforming; direct reduced iron

摘    要:通过CH4-H2-CO-H2O-CO2-O2煤气体系的热力学模拟计算,对焦炉煤气自重整技术进行了研究。结果表明:高温、高CH4含量以及低压有利于焦炉煤气自重整。在配氧量14%,反应温度850~900℃,体系压力为0.3MPa的条件下,对焦炉煤气进行自重整,则还原气平衡态组分中的氢气的体积分数可由60.0%提高到71.5%,CO体积分数可由8.0%提高到23.1%;气体的还原势为97.2%,还原气体总量约增加33%。

Abstract: The technology of self-reforming of coke oven gas was studied by thermodynamics calculation of CH4-H2-CO-H2O-CO2-O2 system.The results show that higher temperature,lower pressure and higher CH4 content are advantage for the self-reforming of COG.With the reforming conditions of 850-900 ℃,0.3 MPa and 14% oxygen,the H2 content of equilibrium system can be enhanced from 60% to 71.5% and 8% to 23.1% for CO.H2+CO/H2O+CO2+H2+CO of equilibrium system is 97.2% and the addition of equilibrium quantity of reducing gas is 33%.

详情信息展示

焦炉煤气自重整炉气成分与温度变化规律研究

曹朝真1,郭培民1,赵沛1,庞建明1

(1.北京市钢铁研究总院先进钢铁流程及材料国家重点实验室)

摘 要:通过CH4-H2-CO-H2O-CO2-O2煤气体系的热力学模拟计算,对焦炉煤气自重整技术进行了研究。结果表明:高温、高CH4含量以及低压有利于焦炉煤气自重整。在配氧量14%,反应温度850~900℃,体系压力为0.3MPa的条件下,对焦炉煤气进行自重整,则还原气平衡态组分中的氢气的体积分数可由60.0%提高到71.5%,CO体积分数可由8.0%提高到23.1%;气体的还原势为97.2%,还原气体总量约增加33%。

关键词:焦炉煤气; 自重整; 直接还原铁

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号