Influence of Ti Powder Characteristics on the Mechanical Properties of Porous Ti Using Space Holder Technique
来源期刊:Acta Metallurgica Sinica2014年第2期
论文作者:Boqiong LI Xing LU
文章页码:338 - 346
摘 要:Porous Ti samples were fabricated by powder metallurgy technique using three kinds of Ti powder and the space holder of polymethyl methacrylate.The final morphological features and mechanical properties were described.Results show that there is only a-Ti phase in porous Ti samples.After sintering,the oxygen content of three porous Ti is increased from the range of 0.34–0.63 wt% to 0.95–1.3 wt%.The porous Ti prepared from the uneven powders with an average particle size of(22.75±11.09) lm presents the largest micro-pore size,grain size,and oxygen content,which lead to the lowest strength and Young’s modulus.
Boqiong LI,Xing LU
Liaoning Key Materials Laboratory for Railway,School of Materials Science and Engineering,Dalian Jiaotong University
摘 要:Porous Ti samples were fabricated by powder metallurgy technique using three kinds of Ti powder and the space holder of polymethyl methacrylate.The final morphological features and mechanical properties were described.Results show that there is only a-Ti phase in porous Ti samples.After sintering,the oxygen content of three porous Ti is increased from the range of 0.34–0.63 wt% to 0.95–1.3 wt%.The porous Ti prepared from the uneven powders with an average particle size of(22.75±11.09) lm presents the largest micro-pore size,grain size,and oxygen content,which lead to the lowest strength and Young’s modulus.
关键词: