摘    要:To study the internal damage of concrete under freeze-thaw cycles, concrete strains were measured using embedded strain gauges. Residual strain and coefficients of freezing expansion (CFE) derived from strain-temperature curves were used to quantify the damage degree. The experimental results show that irreversible residual strain increases with the number of freeze-thaw cycles. After 50 cycles, residual strains of C20 and C35 concretes are 320με and 100με in water, and 120 με and 60 με in saline solution, respectively. In lower temperature range (-10 ℃ to -25 ℃) CFE of C20 and C35 concretes decrease by 9.82×10-6/K and 8.44×10-6/K in water, and 9.38×10-6/K and 5.47×10-6/K in saline solution, respectively. Both residual strains and CFEs indicate that during the first 50 freeze-thaw cycles, the internal damage of concrete in saline solution is less than that of concrete in water. Thus residual strain and CFE can be used to measure the frost damage of concrete.

详情信息展示

Evolution and Characterization of Damage of Concrete under Freeze-thaw Cycles

王玲,CAO Yin,WANG Zhendi,DU Peng

State Key Laboratory of Green Building Materials, China Building Materials Academy

摘 要:To study the internal damage of concrete under freeze-thaw cycles, concrete strains were measured using embedded strain gauges. Residual strain and coefficients of freezing expansion (CFE) derived from strain-temperature curves were used to quantify the damage degree. The experimental results show that irreversible residual strain increases with the number of freeze-thaw cycles. After 50 cycles, residual strains of C20 and C35 concretes are 320με and 100με in water, and 120 με and 60 με in saline solution, respectively. In lower temperature range (-10 ℃ to -25 ℃) CFE of C20 and C35 concretes decrease by 9.82×10-6/K and 8.44×10-6/K in water, and 9.38×10-6/K and 5.47×10-6/K in saline solution, respectively. Both residual strains and CFEs indicate that during the first 50 freeze-thaw cycles, the internal damage of concrete in saline solution is less than that of concrete in water. Thus residual strain and CFE can be used to measure the frost damage of concrete.

关键词:

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号