As-extruded AZ31B Magnesium Alloy Fatigue Crack Propagation Behavior

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2011年第6期

论文作者:张红霞 王文先

文章页码:1114 - 1120

摘    要:The fatigue crack propagation rate of as-extruded AZ31B magnesium alloy was studied. Compact tension [C(T)] of the notch direction parallel (T-L), vertical (L-T), and inclined at 45o to the extrusion direction was investigated. The experimental results indicate that the crack propagation direction is parallel to the extrusion direction for T-L and L-T specimens, whereas the specimen inclined at 45o has an angular deflection of 9° to 11° toward the extrusion direction. The T-L specimen has the fastest fatigue crack propagation rate, and the L-T specimen has the slowest rate, the fatigue crack propagation rate of the specimen inclined at 45o is between the two directions. The crack tip propagates by both transgranular and intergranular fractures. Fatigue fractures consist of cleavage plane or quasi-cleavage and are brittle fractures. The fatigue striation occurs for specimens inclined at 45o and its size is 3-15 μm.

详情信息展示

As-extruded AZ31B Magnesium Alloy Fatigue Crack Propagation Behavior

张红霞,王文先

College of Material Science and Engineering,Taiyuan University of Technology

摘 要:The fatigue crack propagation rate of as-extruded AZ31B magnesium alloy was studied. Compact tension [C(T)] of the notch direction parallel (T-L), vertical (L-T), and inclined at 45o to the extrusion direction was investigated. The experimental results indicate that the crack propagation direction is parallel to the extrusion direction for T-L and L-T specimens, whereas the specimen inclined at 45o has an angular deflection of 9° to 11° toward the extrusion direction. The T-L specimen has the fastest fatigue crack propagation rate, and the L-T specimen has the slowest rate, the fatigue crack propagation rate of the specimen inclined at 45o is between the two directions. The crack tip propagates by both transgranular and intergranular fractures. Fatigue fractures consist of cleavage plane or quasi-cleavage and are brittle fractures. The fatigue striation occurs for specimens inclined at 45o and its size is 3-15 μm.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号