简介概要

Microstructural Characterization and Mechanical Properties of VB2/A390 Composite Alloy

来源期刊:JOURNAL OF MATERIALS SCIENCE TECHNOLOG2015年第10期

论文作者:Xiaoli Cui Yuying Wu Xiangfa Liu

文章页码:1027 - 1033

摘    要:In this work, we make the best use of the vanadium element; a series of Al–V–B alloys and VB2/A390 composite alloys were fabricated. For Al–10V–6B alloy, the grain size of VB2 can be controlled within about 1 μm and is distributed uniformly in the Al matrix. Further, it can be found that VB2 promises to be a useful reinforcement particle for piston alloy. The addition of VB2 can improve the mechanical properties of the A390 composite alloys significantly. The results show that with 1% VB2 addition, A390 composite alloy exhibits the best performance. Compared with the A390 alloy, the coefficient of thermal expansion is 13.2 × 10-6K-1, which decreased by 12.6%; the average Brinell hardness can reach 156.5 HB, wear weight loss decreased by 28.9% and ultimate tensile strength at 25 °C(UTS25 °C) can reach 355 MPa, which increased by 36.5%.

详情信息展示

Microstructural Characterization and Mechanical Properties of VB2/A390 Composite Alloy

Xiaoli Cui,Yuying Wu,Xiangfa Liu

Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials,Ministry of Education,Shandong University

摘 要:In this work, we make the best use of the vanadium element; a series of Al–V–B alloys and VB2/A390 composite alloys were fabricated. For Al–10V–6B alloy, the grain size of VB2 can be controlled within about 1 μm and is distributed uniformly in the Al matrix. Further, it can be found that VB2 promises to be a useful reinforcement particle for piston alloy. The addition of VB2 can improve the mechanical properties of the A390 composite alloys significantly. The results show that with 1% VB2 addition, A390 composite alloy exhibits the best performance. Compared with the A390 alloy, the coefficient of thermal expansion is 13.2 × 10-6K-1, which decreased by 12.6%; the average Brinell hardness can reach 156.5 HB, wear weight loss decreased by 28.9% and ultimate tensile strength at 25 °C(UTS25 °C) can reach 355 MPa, which increased by 36.5%.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号