攀钢2号高炉炉身结瘤形成原因分析

来源期刊:钢铁2010年第1期

论文作者:付卫国

文章页码:10 - 13

关键词:高炉冶炼; 炉身结瘤; ZnO; 形成原因

Key words:blast furnace smelting; stack accretion; ZnO; formation reason

摘    要:攀钢2号高炉于2004年6月开始结瘤,炉身上部炉瘤粘结高度达4~8 m,厚度最大为1.5~1.8 m,对高炉生产造成了严重的影响,高炉被迫停炉处理结瘤。通过对高炉结瘤物进行调查与成因分析,弄清了结瘤形成的原因,提出了预防结瘤的措施:加强烧结原料的管理,减少高ZnO原料入炉。

Abstract: No.2 blast furnace of Pan Steel was found to began accreting since June 2004.Now the height and thickness of accretions in the upper stack were amounted to 4-8m and 1.5-1.8m,respectively.This has seriously decreased the production,so the blast furnace had to blow out to treat the accretions.According to the investigating and analyzing for the accretions,the accretion formation reasons were clarified and prevention measures were put forward.The main measures are intensifying the manage of sinter materials and decreasing the amount of high content of ZnO materials charged into blast furnace.

详情信息展示

攀钢2号高炉炉身结瘤形成原因分析

付卫国1

(1.四川省攀枝花市 攀枝花钢铁研究院)

摘 要:攀钢2号高炉于2004年6月开始结瘤,炉身上部炉瘤粘结高度达4~8 m,厚度最大为1.5~1.8 m,对高炉生产造成了严重的影响,高炉被迫停炉处理结瘤。通过对高炉结瘤物进行调查与成因分析,弄清了结瘤形成的原因,提出了预防结瘤的措施:加强烧结原料的管理,减少高ZnO原料入炉。

关键词:高炉冶炼; 炉身结瘤; ZnO; 形成原因

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号