Selectively recovering scandium from high alkali Bayer red mud without impurities of iron, titanium and gallium

来源期刊:Journal of Rare Earths2017年第9期

论文作者:刘召波 宗燕兵 李宏煦 贾东民 赵子晗

文章页码:896 - 905

摘    要:Experimental results here can give some new insights into the mechanism of selective recovery of scandium and sodium from high alkali Bayer red mud(RM) through sulfation-roasting-leaching process. Effects of roasting and leaching conditions including roasting time, roasting temperature, concentrated H2SO4 addition, leaching temperature, leaching time and liquid to RM solid ratio on the leaching rates of calcium, iron, aluminum, silicon, sodium, titanium, scandium and gallium were studied and analyzed, suggesting that roasting temperature and roasting time were the two primary constraints on selective recovery of Sc and Na. High leaching temperature also brought a negative effect on the iron leaching rate. Phase transitions and thermal behaviors of sulfated RM indicated that sodium had an inhibitory action on the liberation of SO2 or SO3 from metal sulfates, which should follow the decomposition order of TiOSO4>Ga2(SO43>Fe2(SO43>NaFe(SO42>NaAl(SO42Al2(SO43>Na3Sc(SO43>Na2SO4>CaSO4. After water leaching, solid-liquid separation could be carried out extremely smoothly and >95 wt.% Na+, 60 wt.% Sc in [Sc(H2O)x(SO4n]3–2n(x≤6) with impurities of 0 wt.% Fe3+, 0 wt.% Ti4+, 0 wt.% Ga3+, 7 wt.% Al3+, 29 wt.% Ca2+ and 3 wt.% Si4+ could be leached into leachant under the optimized roasting and leaching conditions. The alkali-free residue obtained could then be employed as iron-making or building materials.

详情信息展示

Selectively recovering scandium from high alkali Bayer red mud without impurities of iron, titanium and gallium

刘召波,宗燕兵,李宏煦,贾东民,赵子晗

School of Metallurgical and Ecological Engineering University of Science and Technology Beijing

摘 要:Experimental results here can give some new insights into the mechanism of selective recovery of scandium and sodium from high alkali Bayer red mud(RM) through sulfation-roasting-leaching process. Effects of roasting and leaching conditions including roasting time, roasting temperature, concentrated H2SO4 addition, leaching temperature, leaching time and liquid to RM solid ratio on the leaching rates of calcium, iron, aluminum, silicon, sodium, titanium, scandium and gallium were studied and analyzed, suggesting that roasting temperature and roasting time were the two primary constraints on selective recovery of Sc and Na. High leaching temperature also brought a negative effect on the iron leaching rate. Phase transitions and thermal behaviors of sulfated RM indicated that sodium had an inhibitory action on the liberation of SO2 or SO3 from metal sulfates, which should follow the decomposition order of TiOSO4>Ga2(SO43>Fe2(SO43>NaFe(SO42>NaAl(SO42Al2(SO43>Na3Sc(SO43>Na2SO4>CaSO4. After water leaching, solid-liquid separation could be carried out extremely smoothly and >95 wt.% Na+, 60 wt.% Sc in [Sc(H2O)x(SO4n]3–2n(x≤6) with impurities of 0 wt.% Fe3+, 0 wt.% Ti4+, 0 wt.% Ga3+, 7 wt.% Al3+, 29 wt.% Ca2+ and 3 wt.% Si4+ could be leached into leachant under the optimized roasting and leaching conditions. The alkali-free residue obtained could then be employed as iron-making or building materials.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号