REMAINING LIFE ASSESSMENT OF A 1Cr5Mo STEEL BY USING Z-PARAMETER METHOD

来源期刊:Acta Metallurgica Sinica2004年第4期

论文作者:S.Q.Han S.M.Xie H.B.Gao J.Zhao L.Wang

Key words:life assessment; spheroidization; carbides; creep rupture;

Abstract: Z-parameter method based on the Larson-Miller relationship is proposed to assess remaining life of a 1Cr5Mo steel. The non-linear master curve of stress σ vs. LarsonMiller parameter P of the steel can be expressed as: P=29.608-5.0851ogσ. A family of curves parallel to the master curve can be expressed as: P=29.608-Z-5.0851ogσ,where the value of Z represents the magnitude deviated from the master curve. A relationship between the value of Z-parameter and the level of spheroidization E (microstructural degradation) can be expressed as: Z=0.203(E-1).

详情信息展示

REMAINING LIFE ASSESSMENT OF A 1Cr5Mo STEEL BY USING Z-PARAMETER METHOD

S.Q.Han1,S.M.Xie1,H.B.Gao1,J.Zhao1,L.Wang1

(1.Department of Materials Engineering, Dalian University of Technology, Dalian 116024, China)

Abstract:Z-parameter method based on the Larson-Miller relationship is proposed to assess remaining life of a 1Cr5Mo steel. The non-linear master curve of stress σ vs. LarsonMiller parameter P of the steel can be expressed as: P=29.608-5.0851ogσ. A family of curves parallel to the master curve can be expressed as: P=29.608-Z-5.0851ogσ,where the value of Z represents the magnitude deviated from the master curve. A relationship between the value of Z-parameter and the level of spheroidization E (microstructural degradation) can be expressed as: Z=0.203(E-1).

Key words:life assessment; spheroidization; carbides; creep rupture;

【全文内容正在添加中】

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号