Diffusion welding process and joint’s microstructure behavior of SiC_w/6061Al composite

来源期刊:Rare Metals2004年第4期

论文作者:LIU Liming, DONG Changfu, and GAO Zhenkun Department of Materials Engineering, Dalian University of Technology, Dalian , China National Key Laboratory For Precision Hot Processing of Metals, Harbin Institute of Technology, Harbin , China

文章页码:347 - 351

摘    要:<正>The rules such as process parameters affecting joint properties and the evolution principle of weld’s microstructure have been researched by adopting diffusion welding process to connect SiCw/6061Al composite. Experimental results show that there exists a critical temperature region between solid and liquid phase line of SiCw/6061 Al composite, and the region will shrink with the increasing of welding pressure. When diffusion welding occurred under the critical temperature region, welding joint exhibits bad property of bonding, and the matrix and the reinforcement can’t bond effectively. When diffusion welding occurred in the critical temperature region, the strength of welding joint changes widely with the variation of welding temperature. When welding temperature varies in 10癈, the strength of welding joint will change obviously. Only when welding temperature is higher than the critical temperature region, stable joint properties can be obtained. Simultaneously the matrix and the reinforcement has bet

详情信息展示

Diffusion welding process and joint’s microstructure behavior of SiC_w/6061Al composite

LIU Liming, DONG Changfu, and GAO Zhenkun Department of Materials Engineering, Dalian University of Technology, Dalian 116024, China National Key Laboratory For Precision Hot Processing of Metals, Harbin Institute of Technology, Harbin 15001, China

摘 要:<正>The rules such as process parameters affecting joint properties and the evolution principle of weld’s microstructure have been researched by adopting diffusion welding process to connect SiCw/6061Al composite. Experimental results show that there exists a critical temperature region between solid and liquid phase line of SiCw/6061 Al composite, and the region will shrink with the increasing of welding pressure. When diffusion welding occurred under the critical temperature region, welding joint exhibits bad property of bonding, and the matrix and the reinforcement can’t bond effectively. When diffusion welding occurred in the critical temperature region, the strength of welding joint changes widely with the variation of welding temperature. When welding temperature varies in 10癈, the strength of welding joint will change obviously. Only when welding temperature is higher than the critical temperature region, stable joint properties can be obtained. Simultaneously the matrix and the reinforcement has bet

关键词:

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号