Fe-Sn偏晶合金的深过冷快速凝固组织

来源期刊:中国有色金属学报2003年第2期

论文作者:朱定一 杨晓华 韩秀君 魏炳波

文章页码:328 - 334

关键词:偏晶合金; 深过冷; 落管; 共生组织; 平界面生长

Key words:monotectic alloy; deep undercooling; drop tube; coupled growth structure; planar interface growth

摘    要:采用3m落管实验装置研究了Fe-Sn偏晶合金深过冷快速凝固组织。 结果显示在大的过冷度下, 亚偏晶合金, 偏晶合金和过偏晶Fe-Sn合金均获得了组织均匀的两相共生组织, 表明在过冷条件下偏晶相图具有与共晶相图相似的偏晶共生区。在过偏晶合金中, 富Sn液相优先聚集生长, 具有调幅分解生长特征; 而在亚偏晶合金中, 领先形成相为Fe的固溶体, 它以形核长大的方式进行。 在Fe-26.2%Sn亚偏晶合金中, 首次获得了绝对稳定平界面生长单相组织, 实际的溶质分配系数kV→1, 经计算, 获得绝对稳定平界面生长的临界过冷度为588K, ΔT=0.4TL, 对应的生长速度为38.3m/s。

Abstract: The rapid solidification microstructures of Fe-Sn alloys at deep undercooling were studied by using 3m drop tube facility. The results show that the disperse microstructures of coupled growth of two phases are obtained in hypomonotectic, monotectic and hypermonotectic alloys under deep undercooling condition. It indicates that there is a monotectic coupled growth zone in monotectic phase diagram at deep undercooling condition, which is similar to that in eutectic phase diagram. Sn-rich liquid phase forms and grows firstly in hypermonotectic alloy, which grows in way of spinodal. The Fe solution forms firstly in hypomonotectic alloys, which grows in way of nucleation and growth. The absolute stable monophase microstructure with planar interface was obtained at first time in Fe-26.2%Sn hypomonotectic alloy with the real distributive coefficient of solute, kV, is close to 1. It is calculated that the critical undercooling of the alloy in growth way of absolute stable planar interface is 588K and its growth velocity is 38m/s. The critical undercooling is 0.4 times of the melt temperature of the alloy.

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号