Study on Roasting Decomposition of Mixed Rare Earth Concentrate in CaO-NaCl-CaCl2

来源期刊:JOURNAL OF RARE EARTHS2006年增刊第2期

论文作者:Sun Shuchen Bian Xue Wu Wenyuan Tu Ganfeng

Key words:mixed rare earth concentrate; roasting; CaO-CaCl-CaCl2;

Abstract: The decomposed process of bastnaesite, monazite and mixed rare earth concentrate in CaO-CaCl-CaCl2 was studied by means of TG-DTA method. The relationship among decomposition ratio, roasting temperature, and CaO-NaCl addition was studied by the quadratic regression orthogonal analysis, and then the regression equation was obtained. Through analysis, the optimum process conditions of mixed rare earth concentrate decomposed by CaO-CaCl-CaCl2 were obtained as follows: roasting temperature: 700 ℃, CaO addition: 15%, NaCl-CaCl2 addition: 10%, roasting time: 60 min, the decomposition ratio: 91.3%.

详情信息展示

Study on Roasting Decomposition of Mixed Rare Earth Concentrate in CaO-NaCl-CaCl2

Sun Shuchen1,Bian Xue1,Wu Wenyuan1,Tu Ganfeng1

(1.School of Materials & Metallurgy, Northeastern University, Shenyang 110004, China)

Abstract:The decomposed process of bastnaesite, monazite and mixed rare earth concentrate in CaO-CaCl-CaCl2 was studied by means of TG-DTA method. The relationship among decomposition ratio, roasting temperature, and CaO-NaCl addition was studied by the quadratic regression orthogonal analysis, and then the regression equation was obtained. Through analysis, the optimum process conditions of mixed rare earth concentrate decomposed by CaO-CaCl-CaCl2 were obtained as follows: roasting temperature: 700 ℃, CaO addition: 15%, NaCl-CaCl2 addition: 10%, roasting time: 60 min, the decomposition ratio: 91.3%.

Key words:mixed rare earth concentrate; roasting; CaO-CaCl-CaCl2;

【全文内容正在添加中】

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号