Catalytic Oxidative Properties and Characterization of CuO/CeO2 Catalysts

来源期刊:JOURNAL OF RARE EARTHS2003年第1期

论文作者:蒋晓原 吕光烈 周仁贤 袁骏 郑小明

Key words:physical chemistry; CuO/CeO2 catalysts; CO micro-reactor GC system; rare earths;

Abstract: The oxidative properties and characterization of CuO, CeO2 and CuO/CeO2 catalysts were examined by means of a CO micro-reactor GC system, TPR, XPS and X-ray diffraction Rietveld methods. The results show that either CuO or CeO2 activity is quite low for CO oxidation. However, when CuO and CeO2 are mixed, the oxidative activity of the catalyst increases significantly, probably owing to the valency status of copper species (Cu2+ and Cu+) on the CeO2 surface, the dispersion and reducibility. XPS surface analysis shows that CuO loading is very important in forming of either Cu2+ or Cu+. Rietveld analysis shows that some CuO, which has smaller ion radius than Ce4+, enters the CeO2 lattice after CuO and CeO2 are mixed. When the CuO loading reaches 5.0%, the size of CuO crystals is a minimum (6.1 nm) and the micro-strain value is a maximum (2.86×10-3), resulting in high surface energy and the best activity for CO oxidation.

详情信息展示

Catalytic Oxidative Properties and Characterization of CuO/CeO2 Catalysts

蒋晓原1,吕光烈2,周仁贤1,袁骏3,郑小明1

(1.Institute of Catalysis;
2.Analysis and Test Center, Zhejiang University, Hangzhou 310028, China;
3.State Key Laboratory of Silicon Material Science)

Abstract:The oxidative properties and characterization of CuO, CeO2 and CuO/CeO2 catalysts were examined by means of a CO micro-reactor GC system, TPR, XPS and X-ray diffraction Rietveld methods. The results show that either CuO or CeO2 activity is quite low for CO oxidation. However, when CuO and CeO2 are mixed, the oxidative activity of the catalyst increases significantly, probably owing to the valency status of copper species (Cu2+ and Cu+) on the CeO2 surface, the dispersion and reducibility. XPS surface analysis shows that CuO loading is very important in forming of either Cu2+ or Cu+. Rietveld analysis shows that some CuO, which has smaller ion radius than Ce4+, enters the CeO2 lattice after CuO and CeO2 are mixed. When the CuO loading reaches 5.0%, the size of CuO crystals is a minimum (6.1 nm) and the micro-strain value is a maximum (2.86×10-3), resulting in high surface energy and the best activity for CO oxidation.

Key words:physical chemistry; CuO/CeO2 catalysts; CO micro-reactor GC system; rare earths;

【全文内容正在添加中】

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号