TC21合金片层组织特征对其断裂韧性的影响

来源期刊:中国有色金属学报2010年第z1期(上册)

论文作者:党薇 薛祥义 李金山 胡锐 朱知寿 张丰收 周廉

文章页码:16 - 20

关键词:TC21钛合金;片层组织特征;断裂韧度

Key words:TC21 alloy; lamellar microstructure feature; fracture toughness

摘    要:研究TC21合金经β相区固溶并慢速冷却后的片层组织特征(晶界α层厚度、α片层宽度、α集束尺寸)及断裂韧度随冷却速率的变化规律,探讨片层组织特征与断裂韧度的关系。结果表明:随着冷却速率的增大,TC21合金α片层集束、α片层厚度及晶界α层宽度均减小。在本文实验测试尺度范围内,α片层宽度、α片层集束尺寸及晶界α层厚度的增大均可提高合金的断裂韧性。

Abstract: In order to analyze the relationship between lamellar microstructure feature (thickness of α laths, width of α lath at grain boundary and α colony size) and fracture toughness, the microstructures and fracture toughness of TC21 alloy cooled from β phase field with different slow rates were investigated. The results show that α colony size together with α laths thickness and width of α lath at grain boundary is decreased with increasing cooling rates, leading to the decrease of fracture toughness. It is positive for fracture toughness to decrease width of α lath at grain boundary, α laths thickness and α colony size.

基金信息:国家重点基础研究发展计划资助项目

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号